Effect of Hydrofluoric Acid Etching Surface Treatment of Zirconia on the Shear Bond Strength with Resin Cement

Department of Prosthodontics, Oral Science Research Center, College of Dentistry, Yonsei University, Seoul, 03722, Korea

Corresponding Author: You-Jung Kang, E-mail: kyj1219@yonsei.ac.kr

Volume 9, Number 2, Pages 79–86, June 2021.
Korean J Clin Dent Hyg 2021;9(2):79–86. https://doi.org/10.12972/kjcdh.20210009
Received on June 09, 2021, Revised on June 21, 2021, Accepted on June 21, 2021, Published on June 30, 2021.
Copyright © 2021 by Korean Society of Infection Control and Prevention in Dental Hygiene.
This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License(http://creativecommons.org/licenses/by-nc/4.0/).

Abstract

Objectives: The purpose of this study was to investigate the effect of hydrofluoric (HF) acid surface treatment of zirconia on its shear bond strength (SBS) with resin cement. Methods: Based on the surface treatment method, 52 zirconia specimens were divided into four groups which were airborne-particle abrasion treatment group (APA), 9% HF acid etching group (HFE), the group with 9% HF acid gel with hot etching performed once (HFHE1), and the group with 9% HF acid gel with hot etching performed twice (HFHE2). After the primer was applied to the specimens of each group, the resin cement adhered to the zirconia. Thereafter, the SBS was measured using a universal testing machine. The surface of the representative specimens of each group was observed using a scanning electron microscope (SEM). SBS was performed, followed by statistical analysis of the result using One-way ANOVA (α=0.05). Results: The HFHE1 group showed a significant difference in SBS compared with the other groups. The SEM analysis found a change in the surface morphology for all surface-treated samples. Conclusions: Within the limits of this study, surface treatment with low-concentration of HF acid hot etching formed a uniform microporous structure on the zirconia surface and exhibited high SBS.
Keywords

불산, 전단결합강도, 표면처리, 지르코니아, Hydrofluoric acid, Shear bond strength, Surface treatment, Zirconia,